IEEE Transactions on Electron Devices · 1996 · 60 citations · 29 references
EngineeringElectrical EngineeringMicroelectronicsQuality EngineeringSemiconductor DevicesDevice CharacterizationDevice ModelingDevice ReliabilityFailure AnalysisFailure CriteriaSemiconductor ReliabilityBreakdown VoltageBreakdown Voltage TestingGate Oxide DegradationGate Oxide ReliabilityLifetime EstimationLifetime TestingOxide ReliabilityThinning
This paper compares several popular accelerated test methods for projecting SiO/sub 2/ lifetime distribution or failure rate: constant-voltage and constant-current time-to-breakdown and charge-to-breakdown tests, ramp-voltage breakdown test, and ramp-current charge to-breakdown test. Charge trapping affects the electric field acceleration parameter for time-to-breakdown and the value of breakdown voltage. Practical considerations favor ramp breakdown testing for gate oxide defect characterization. The effective thinning model is used for defect characterization and the ramp-voltage breakdown test is shown to be superior to the ramp-current Q/sub BD/ test for extraction of the defect distribution. Measurement issues are also discussed.
29