Natural SciencesMaterials EngineeringMaterials ScienceOptical MaterialsOptoelectronicsSemiconductor MaterialsInfrared Optical MaterialsLuminescent MaterialsOptical Properties Of SemiconductorsOptoelectronic MaterialsRare-earth-doped MaterialsSilicon MaterialsCrystalline StructurePhotoluminescencePhotoluminescence SpectroscopyRapid Thermal OxidationRare-earth-doped Luminescent MaterialsSemiconductor Infrared MaterialsThermal OxidationWet Chemical Synthesis
Optically active and electrically excitable erbium complexes on silicon are made by wet-chemical synthesis. The single-crystalline Er–Si–O compound is formed by coating a Si(100) substrate with an ErCl3∕ethanol solution, followed by rapid thermal oxidation and annealing. Room-temperature Er-related 1.53μm photoluminescence is observed with a peak linewidth as small as 4meV. The complexes can be excited directly into the Er intra-4f states, or indirectly, through photocarriers. Er concentrations as high as 14at.% are achieved, incorporated in a crystalline lattice with a 0.9nm periodicity. Thermal quenching at room temperature is only a factor 5, and the lifetime at 1.535μm is 200μs.
11
Minoru Fujii, Masato Yoshida, Yoshihiko Kanzawa et al. · Applied Physics Letters · 1997 · 537 citations
Natural Sciences, Materials Engineering, Materials Science +17