Journal of Applied Physics · 1988 · 151 citations · 29 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor MaterialsThin FilmsChemical Vapor DepositionDefects In Electronic MaterialsDislocations In SemiconductorsSemiconductor DefectsSemiconductor PhysicsSilicon MaterialsBand GapCrystal PerfectionEpitaxial Thin FilmsExtended DefectsFilm StressFilm ThicknessPhotoluminescenceStress
26 cubic SiC (3C-Sic) films grown on (100) Si by way of chemical vapor deposition (CVD) with SiC film thicknesses ranging from 600 Å to 25 μm have been studied by photoluminescence at 2 K. The ‘‘defect-related’’ W band near 2.15 eV appears in very thin-film samples. The G band near 1.90–1.92 eV and its phonon side bands G1 and G2 are believed to be related to dislocations and extended defects. The ratio ρ of the intensities of the G band and the strongest nitrogen-bound exciton (N-BE) TO(X) line may be used as a figure of merit for crystalline perfection in CVD 3C-SiC films. General formulas for the band-gap shift due to an axial stress, including three special cases—hydrostatic pressure and uniaxial and biaxial stress—are derived and applied to the CVD 3C-SiC/Si system. An experimental relationship of stress in these epitaxial films of 3C-SiC as a function of depth is obtained. It is shown that a 1–3 μm transition layer greatly reduces the interface misfit strain. For films thicker than 3 μm the film stress decreases slightly with increase of film thickness. The effects of biaxial stress on the relative intensities of N-BE lines are experimentally studied. It is reported that biaxial stress in the SiC/Si system depresses the intensity of the no-phonon line as well as the TA, LA, and LO phonon transitions of the N-BE spectrum.
29
Piezo-Electroreflectance in Ge, GaAs, and Si
Fred H. Pollak, M. Cardona · Physical Review · 1968 · 852 citations
Natural Sciences, Materials Engineering, Materials Science +16