Journal of the American Chemical Society · 2006 · 44 citations · 17 references
Natural SciencesMaterials EngineeringMaterials ScienceMaterials ChemistrySurface ScienceThin FilmsAtomic Layer DepositionSurface OxidationSurface PhysicsThin Film OxidationThin-film DepositionThin-film MaterialsDeposition CyclesElastic RecoilFilm ThicknessGrowth RatesPrecursor Chemical ControlPrecursor ChemistryThin Oxide FilmsThin-film Growth Kinetics
The atomic layer deposition of W2O3 films was demonstrated employing W2(NMe2)6 and water as precursors with substrate temperatures between 140 and 240 degrees C. At 180 degrees C, surface saturative growth was achieved with W2(NMe2)6 vapor pulse lengths of >/=2 s. The growth rate was about 1.4 A/cycle at substrate temperatures between 140 and 200 degrees C. Growth rates of 1.60 and 2.10 A/cycle were observed at 220 and 240 degrees C, respectively. In a series of films deposited at 180 degrees C, the film thicknesses varied linearly with the number of deposition cycles. Time-of-flight elastic recoil analyses demonstrated stoichiometric W2O3 films, with carbon, hydrogen, and nitrogen levels between 6.3 and 8.6, 11.9 and 14.2, and 4.6 and 5.0 at. %, respectively, at substrate temperatures of 160, 180, and 200 degrees C. The as-deposited films were amorphous. Atomic force microscopy showed root-mean-square surface roughnesses of 0.7 and 0.9 nm for films deposited at 180 and 200 degrees C, respectively. The resistivity of a film grown at 180 degrees C was 8500 microhm cm.
17
Lauri Niinist�, Minna Nieminen, J. P�iv�saari et al. · physica status solidi (a) · 2004 · 339 citations
Natural Sciences, Materials Engineering, Materials Science +17