2006 1st Electronic Systemintegration Technology Conference · 2006 · 20 citations · 13 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMaterials CharacterizationMetallic MaterialsAlloysCreep BehaviorCreep DeformationMetalsWork HardeningAlloy Composition EffectsAlloy Creep BehaviorCreep AgingCreep MechanismsMetal Alloy CompositionSoldered JointsSolderingSoldering Joints
The paper presents creep data, that was gained on non eutectic SnAgCu-solder specimens with a variety of compositions. The non eutectic SnAgCu-alloys were tested in different specimen sizes: bulk specimens, FBGA solder balls, flip chip solder joints. The results of the creep experiments show that both solder alloy composition and solder joint size have a significant influence of the creep properties of the solder material. Bulk solder specimens have a rectangular cross section of 4mm times 3mm and contained the following alloys: Sn98Ag2, Sn97Ag3, Sn96Ag4, Sn97.5Ag2Cu0.5, Sn97.1Ag2Cu0.9, Sn98.8Ag2Cu1.2, Sn96.5Ag3Cu0.5, Sn96.1Ag3Cu0.9, Sn95.8Ag3Cul.2, Sn96.9Ag3Au0.1. FBGA solder balls contained three noneutectic alloys with a content of 0.5% < Ag < 4% and 0.2% < Cu < 0.8%. Flip chip solder joints contained eutectic Sn96.5Ag3.5 alloy and an non-eutectic SnAg alloy with Ag < 3%. Creep experiments have been carried out in a temperature range between T = 5degC ... 150degC. The microstructures of the various solder specimens have been analysed to understand their differences in creep behavior
13