Physical review. B, Solid state · 1977 · 297 citations · 17 references
Natural SciencesMaterials SciencePhysicsCondensed Matter PhysicsElectronic MaterialsSemiconductor MaterialsDefectsDefects In Electronic MaterialsDopingRadiation Damage In MaterialsSemiconductor DefectsSilicon MaterialsAnnealingDefect Energy LevelsDefect LevelsDefect PhysicsImpurity DefectsInterstitial DefectsSiliconSilicon Defects
Using transient capacitance spectroscopy, we studied defect energy levels and their annealing behavior in boron-doped silicon of various resistivities irradiated with 1-MeV electrons at room temperature. Three levels located at ${E}_{v}+0.23$, ${E}_{v}+0.38$, and ${E}_{c}\ensuremath{-}0.27$ eV consistently appear in various samples, showing they are characteristic defects in boron-doped silicon. Many properties of the ${E}_{v}+0.23$-eV level and the divacancy are the same, according to the present study and others. We correlated the ${E}_{v}+0.38$-eV level to the vacancy-oxygen-carbon complex recently identified by Lee and Corbett using the EPR technique. The ${E}_{c}\ensuremath{-}0.27$-eV level could arise from an interstitial defect of oxygen and boron; and a new level at ${E}_{v}+0.30$ eV arising upon its disappearance could be a vacancy defect trapping an oxygen atom and a boron. Several additional defect levels are reported.
17
RADIATION DAMAGE IN SEMICONDUCTORS.
P. Baruch · Defense Technical Information Center (DTIC) · 1963 · 564 citations
Radiation Damage and Defects in Semiconductors
G Carter · Physics Bulletin · 1973 · 380 citations · Full text