EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsMicrofabricationSemiconductor DevicesElectron Beam LithographyElectron MicroscopyEtching ProcessesFabrication MaterialsMicrofabrication MaterialsSilicon MaterialsReactive Ion EtchingResist PatterningScanning Electron MicroscopyScanning Electron Microscopy AnalysisSiliconSilicon EtchingSilicon Wafer ProcessingThin Film Resist Processing
The present limit of around 10 nm for the width of lines fabricated by e-beam lithography using polymethylmethacrylate (PMMA) resist on silicon substrates has been overcome. 5–7 nm wide etched lines in bulk Si substrates have been produced. A 65 nm thick layer of PMMA was exposed with an 80 kV electron beam of diameter smaller than 5 nm. After exposure the resist was developed in 3:7 cellosolve:methanol with ultrasonic agitation. The pattern in resist was transferred to the Si substrate with reactive ion etching. Lines of width varying between 5 and 7 nm were recorded using an S-900 scanning electron microscope which has a resolution of 0.7 nm.
3
10-nm linewidth electron beam lithography on GaAs
H. G. Craighead, Richard Howard, L. D. Jackel et al. · Applied Physics Letters · 1983 · 138 citations