EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor DevicesSemiconductor MaterialsChemical Vapor DepositionDislocations In SemiconductorsEtching ProcessesSemiconductor Device MaterialsSemiconductor HeterostructuresSemiconductor PhysicsAnnealingDislocation DensityDislocation Density EvolutionLattice MismatchLattice Mismatch StrainMetalorganic Chemical Vapor DepositionStrained-layer HeterostructuresThermal Annealing
GaAs was grown on a Si substrate by metalorganic chemical vapor deposition using GaAs/GaAsP strained-layer superlattice (SLS) intermediate layers. The dislocation density decreases at the interface between GaAs and the SLS, but does not decrease in the SLS. When a GaAs/GaAsP SLS is used as the intermediate layer, part of the threading dislocation propagates into the top GaAs layer because of the lattice mismatch of GaAs and SLS. The low etch pit density of (3–5)×105 cm−2 was obtained by using the intermediate layer of a GaAs/GaAsP SLS and an AlAs/GaAs superlattice with thermal cycle annealing.
7
Defects in epitaxial multilayers
J. W. Matthews, A. E. Blakeslee · Journal of Crystal Growth · 1974 · 1.5K citations