Natural SciencesMaterials EngineeringMaterials ScienceElectrochemistrySurface ScienceThin FilmsDielectricsThin Film AnnealingThin Film Electrical PropertiesThin Film Surface MorphologyThin-film DepositionThin-film MaterialsAnnealingCapacitanceCapacitance-voltage RelationsCurrent DensityDielectric ConstantLattice EnergyLeakage CurrentRare-earth Oxides
thin films with a high dielectric constant (high k value) deposited on n-Si(100) were investigated. A capacitance equivalent thickness of 1.6 nm with a leakage current density of was obtained for 4.5 nm thick deposited at room temperature followed by postdeposition annealing (PDA) at 400°C in The surface morphology for 8-20 nm thick films became rough after the PDA process because of the crystallization, whereas the surface of 4.5 nm thick was smooth even after the PDA process. No frequency dependence in the capacitance-voltage curve was observed, and its relative dielectric constant was 11. The hygroscopic properties of the thin films seemed to be superior to those of other rare-earth oxide thin films, probably due to having the largest lattice energy among the rare-earth oxides. © 2004 The Electrochemical Society. All rights reserved.
13
Dielectric polarizabilities of ions in oxides and fluorides
R. D. Shannon · Journal of Applied Physics · 1993 · 2.8K citations