Integration of Ferroelectric Al0.8Sc0.2N on Si (001) Substrate

Wenxin Sun, Jiuren Zhou, Ning Liu, Siying Zheng, Xiaoxi Li, Bochang Li, Yan Liu, Yue Hao, Genquan Han

IEEE Electron Device Letters · 2024 · 14 citations · 22 references

Concepts

Abstract

We evidently present the integration of ferroelectric Al <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$_{{0}.{8}}$ </tex-math></inline-formula> Sc <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$_{{0}.{2}}\text{N}$ </tex-math></inline-formula> onto a (001)-oriented silicon (Si) substrate. Our AlScN film, having a thickness of 116 nm, shows a remnant polarization ( <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">${P}_{\text {r}}{)}$ </tex-math></inline-formula> exceeding <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$124.5~\mu \text{C}$ </tex-math></inline-formula> /cm2 and a coercive voltage of 71.9 V. Our ferroelectric Al <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$_{{0}.{8}}$ </tex-math></inline-formula> Sc <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$_{{0}.{2}}\text{N}$ </tex-math></inline-formula> on Si demonstrates an endurance performance, surpassing <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$1\times 10^{{4}}$ </tex-math></inline-formula> cycles under a stress of 75 V @ 100 kHz. The extrapolation of retention properties reveals that a substantial <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$2{P}_{\text {r}}$ </tex-math></inline-formula> over <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$200~\mu \text{C}$ </tex-math></inline-formula> /cm2 can be guaranteed for a duration over <inline-formula xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink"> <tex-math notation="LaTeX">$10^{{8}}$ </tex-math></inline-formula> seconds at 300 K. Furthermore, the evaluation of the ratio of breakdown voltage to coercive voltage yields approximately 112% @ 300 K and 131% @ 500 K. These findings mark a critical advancement in the practical implementation of wurtzite ferroelectric field-effect transistor-structural memories and their high-density integration.

References

22