1999 · 17 citations · 6 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsInterface ScienceThin FilmsElectrical ConductivityMetal Oxide NanomaterialsMetalsOxide SemiconductorsThin Film Electrical PropertiesThin-film MaterialsConductionContact DegradationContact MaterialsContact ResistanceMetallic ConductivityPercolationThin Oxide FilmsTin Oxides
A series of experiments were conducted to characterize oxide films that develop during fretting degradation. It was found that while the rate of change in resistance depends on contact force, the oxide film characteristics depend strongly on the number of fretting cycles. Moreover, after about 1000 fretting cycles, the oxygen content reaches a saturation level which corresponds to tin volume fractions below the percolation limit for metallic conduction (<0.4). Consequently, it is concluded that conduction is primarily due to the semiconductor properties of tin oxide (SnO). In addition, sub-micron size particles, composed of tin and tin oxide, were found dispersed over the surface. These particles had tin fractions near the percolation limit and may play a role in the mechanism that causes short-term discontinuities in contact resistance.
6
Scott Kirkpatrick · Reviews of Modern Physics · 1973 · 5.2K citations
Structural and electrical properties of granular metal films
B. Abeles, Ping Sheng, M. D. Coutts et al. · Advances In Physics · 1975 · 1.4K citations
Impact of fretting parameters on contact degradation
R.D. Malucci · 2002 · 53 citations