Thin Film Co<sub>3</sub>O<sub>4</sub>/TiO<sub>2</sub> Heterojunction Solar Cells

Benjamin Kupfer, Koushik Majhi, David A. Keller, Yaniv Bouhadana, Sven Rühle, Hannah Noa Barad, Assaf Y. Anderson, Arie Zaban

Advanced Energy Materials · 2014 · 99 citations · 30 references

Concepts

TL;DR

Co₃O₄ is studied as a light absorber for all‑oxide thin‑film photovoltaic cells because its optical bandgap of ~1.5 eV is nearly ideal. The TiO₂/Co₃O₄ heterojunctions are fabricated by spray‑pyrolyzed TiO₂ as a window layer followed by pulsed‑laser deposition of Co₃O₄, with deposition temperature controlling crystallinity, morphology, and grain size. Device performance increases with Co₃O₄ deposition temperature, reaching a maximum power of 22.7 µW cm⁻², Voc = 430 mV, and Jsc = 0.2 mA cm⁻² at 600 °C, an order‑of‑magnitude improvement over room‑temperature deposition and a reduction in tail states.

Abstract

Co 3 O 4 is investigated as a light absorber for all‐oxide thin‐film photovoltaic cells because of its nearly ideal optical bandgap of around 1.5 eV. Thin film TiO 2 /Co 3 O 4 heterojunctions are produced by spray pyrolysis of TiO 2 as a window layer, followed by pulsed laser deposition of Co 3 O 4 as a light absorbing layer. The photovoltaic performance is investigated as a function of the Co 3 O 4 deposition temperature and a direct correlation is found. The deposition temperature seems to affect both the crystallinity and the morphology of the absorber, which affects device performance. A maximum power of 22.7 μW cm −2 is obtained at the highest deposition temperature (600 °C) with an open circuit photovoltage of 430 mV and a short circuit photocurrent density of 0.2 mA cm −2 . Performing deposition at 600 °C instead of room temperature improves power by an order of magnitude and reduces the tail states (Urbach edge energy). These phenomena can be explained by larger grains that grows at high temperature, as opposed to many nucleation events that occur at lower temperature.

References

30