IEEE Transactions on Components and Packaging Technologies · 2005 · 82 citations · 11 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMechanical Behavior Of MaterialsMetallic MaterialsAlloysMechanical CharacterizationMetalsPhysical MetallurgyStrength Of MaterialsTensile PropertiesElevated-temperature Material PropertiesSolder Joint StrengthSoldered JointsSolderingSoldering JointsTensile DeformationTensile StrainTensile Testing
Mechanical properties for 95.5Sn–3.8Ag–0.7Cu solder alloy were derived from bulk specimen tensile test and lap shear solder joint tests specimen. The tensile tests were carried out at three temperatures (25 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$^circhbox C$</tex> , 75 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$^circhbox C$</tex> , and 125 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$ ^circhbox C$</tex> ) and at three different strain rates ( <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$5.6times 10^-4 hbox s^-1$</tex> , <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$5.6times 10^-3$</tex> and <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$5.6times 10^-2 hbox s^-1$</tex> ). Shear tests were carried out at three temperatures (25 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$ ^circhbox C$</tex> , 75 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$ ^circhbox C$</tex> , and 125 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$ ^circhbox C$</tex> ) and at three different displacement rates (0.5, 0.05, and 0.005 mm/min). The specimen gave the highest strength at the fastest displacement rate and at room temperature of 25 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$ ^circhbox C$</tex> (0.61 Tm). The lowest strength occurs when the specimen is subjected to the slowest displacement rate at elevated temperature of 125 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$ ^circhbox C$</tex> (0.81 Tm). Constant-load creep tests for bulk specimen were also conducted at three different temperatures (25 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$ ^circhbox C$</tex> , 75 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$ ^circhbox C$</tex> , and 125 <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">$ ^circhbox C$</tex> ), test results were compared with other reported data.
11