IEEE Transactions on Components Hybrids and Manufacturing Technology · 1991 · 20 citations · 3 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsInterface ScienceSemiconductor MaterialsAlloysMetalsSemiconductor Device MaterialsThermal Properties Of MaterialsInterface StrengthMicrostructural Interface EvolutionPhase Distribution AnalysisShrinkageThermal CyclesThermal Cycling EffectsTransverse CrackingX-ray Diffraction Analysis
Thermal cycling effects on solder joints between thick-film mixed bonded conductor and Sn/Pb solder are investigated. Microstructural evolution of the interfacial morphology, elemental, and phase distribution are probed with the aid of electron microscopy and X-ray diffraction. Microstructural analysis reveals the formation of intermetallic compounds Pd/sub 3/Sn, Pd/sub 2/Sn, Pd/sub 3/Sn/sub 2/, PdSn, Pd/sub 3/Pb, Ag/sub 5/Sn, and Ag/sub 3/Sn, after thermal cycles from -55 to +125 degrees C. A transverse crack is observed across the joint from the conductor/substrate interface to the conductor/solder interface, which results in the failure of the joint. The microstructural analysis and stress analysis reveal that the transverse crack is initiated by the microcracks at the glass-penetrated region of the substrate and propagates under a tensile stress due to the solder shrinkage. An appropriate joint geometry and a materials system with good interface strength and with negligible thermal expansion mismatch are important in the enhancement of the life time for the solder joints in thick-film microelectronics.< <ETX xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">></ETX>
3
Introduction to Ceramics 2nd ed.
W. D. Kingery, H. Kent Bowen, D. R. Unlmann · 1960 · 1.4K citations
Natural Sciences, Materials Engineering, Materials Science +10