Effect of growth interruption on In‐rich InGaN/GaN single quantum well structures

Soon‐Yong Kwon, Hyun Jin Kim, Hyunseok Na, Hui‐Chan Seo, Yoori Shin, Young‐Woon Kim, Sukho Yoon, Hye Jeong Oh, Cheolsoo Sone, Yongjo Park,

Physica status solidi. C, Conferences and critical reviews/Physica status solidi. C, Current topics in solid state physics · 2003 · 12 citations · 6 references

Concepts

Abstract

We successfully grew In-rich InGaN/GaN single quantum well structures by metal-organic chemical vapor deposition and confirmed their formation by optical and structural measurements. Relatively high growth temperature (730 °C) for InGaN layer facilitated the formation of 2-dimensional quantum well structures, presumably due to high adatom mobility. As the growth interruption time increased, the PL emission efficiency from InGaN layer improved with peak position blue-shifted and the dislocation density decreased by one order of magnitude. The high resolution cross-sectional TEM images clearly showed that the In-rich InGaN layer thickness reduced from 2.5 nm (without GI) to about 1 nm (with 10 s GI) and the InGaN/GaN interface became very flat with 10 s GI. We suggest that decomposition and mass transport processes on InGaN during GI is responsible for these phenomena. (© 2003 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim)

References

6