Journal of the American Ceramic Society · 1981 · 27 citations · 5 references
EngineeringMaterials EngineeringMaterials ScienceCrystal StructureSemiconductor MaterialsThin FilmsAmorphous SemiconductorsChemical Vapor DepositionSemiconductor Crystal GrowthSemiconductor Device MaterialsSemiconductor SurfacesSilicon MaterialsChemical Vapor Deposition MaterialsChemical Vapor Deposition PrecursorsCrystal Preferred OrientationCrystallographic Preferred OrientationLattice ParametersPreferred OrientationSilicon CarbideSilicon Nitride
Beta‐type CVD‐Si 3 N 4 plates (up to 1.1 mm thick) have been prepared by adding TiCl 4 vapor to the system SiCl 4 ‐NH 3 ‐H 2 at deposition temperatures of 1350° to 1450°C, while α‐type or amorphous CVD‐Si 3 N 4 was obtained without TiCl 4 vapor at the same deposition temperature. Three to four wt % 777V was included in the β‐type CVD‐Si 3 N 4 matrix. The density, preferred orientation, and lattice parameters of β‐type CVD‐Si 3 N 4 were examined.
5