Surface Defects in Polished Silicon Studied by Cross‐Sectional Transmission Electron Microscopy

Stefan Johansson, Jan‐Åke Schweitz, K. Peter, O. Lagerlöf

Journal of the American Ceramic Society · 1989 · 33 citations · 15 references

Concepts

Abstract

The cross‐sectional TEM technique is applied to Si(100) surfaces, which are exposed to mild polishing with diamond paste in the 0.25‐ to 6‐μm‐size range as well as with the commercial polishing medium Syton HT 50. Syton polishing is also used to prepare electron‐transparent foils for TEM studies, and this preparation technique shows several advantages over ion thinning. Mild diamond polishing results in small‐scale abrasive grooving and production of superficial dislocation loops of 1/2〈110〉{111} type. Debris of amorphous material tends to aggregate in surface cavities. These aggregates are formed during polishing, not by ion milling. Syton polishing results in very smooth surfaces, with no signs of abrasive grooving or dislocation density. Two major mechanisms of mass removal are suggested: (1) “smearing” of very superficial material at a nearly atomic level, resulting in amorphous aggregates and (2) strongly localized plastic cutting or shearing. In mild polishing, both mechanisms are suggested to be active, localized plastic cuttinglshearing becoming progressively more dominant for increasing particle size.

References

15