Optics Express · 2024 · 10 citations · 28 references
EngineeringMaterials EngineeringMaterials ScienceOptoelectronicsSemiconductor DevicesSemiconductor MaterialsLight-emitting DiodesLuminescent MaterialsOptoelectronic MaterialsSemiconductor Device MaterialsSemiconductor HeterostructuresStrain EngineeringCompressive StrainExternal Quantum EfficiencyGallium Nitride (Gan) MaterialsGallium Nitride Light-emitting DiodesLight-emitting DevicesQuantum EfficiencyRed Light-emitting DiodesSemiconductor Light-emitting Materials
This work proposed to modulate the strain of underlying GaN layers using different thicknesses of sputtered AlN nucleation layer to achieve long-wavelength red InGaN mini-light-emitting diodes (mini-LEDs). The increase in thickness of sputtered AlN from 15 nm to 60 nm could reduce the compressive strain in epitaxial GaN layers, which led to a shift in the peak wavelength of InGaN LEDs ranging from 633 nm to 656 nm at 1 A/cm 2 . However, a significant decrease in external quantum efficiency (EQE) was observed when the sputtered AlN thickness was increased from 45 nm to 60 nm. We found that the EQE and peak wavelength (PW) of the red mini-LEDs with 45-nm sputtered AlN at 1 A/cm 2 were 8.5% and 649 nm, respectively. The study revealed that varying the thickness of AlN nucleation layers could extend the emission of red InGaN mini-LEDs toward longer wavelengths with a slight EQE loss.
28
Strain-related phenomena in GaN thin films
C. Kisielowski, Joachim Krüger, S. Ruvimov et al. · Physical review. B, Condensed matter · 1996 · 886 citations
Natural Sciences, Materials Engineering, Materials Science +17