Amorphous WO3 Films via “Wet” CVD of a WVI Oxoalkoxide Precursor

Marino Basato, E. Brescacin, E. Tondello

Chemical Vapor Deposition · 2001 · 17 citations · 0 references

Concepts

Abstract

Amorphous WO3 films are obtained by using the oxoalkoxide precursor WO(OtBu)4. This compound is easily evaporated at 80 °C, and reacts with water at the surface of the substrate (Si(100) or soda lime glass (KGlass)) to give films of tungsten oxide in a combined CVD sol–gel process. The films deposited at low temperatures (150 °C, Si(100), or 100 °C, KGlass) can be defined as tungstic species (of general formula WOn(OH)m), having interesting electrochromic properties. Thermal treatment at temperatures over 400 °C converts the material to a more typical WO3 film.