Physica Scripta · 2016 · 21 citations · 15 references
Natural SciencesMaterials SciencePhysicsPlasma PhysicsSpectroscopySurface ScienceHigh-temperature PlasmasPlasma Surface TreatmentPlasma-surface InteractionsRadiation Damage In MaterialsSurface PhysicsSurface SpectroscopyEnergy DensityPlasma Exposure EffectsPlasma Exposure TestingPlasma-induced DamagePlasma-induced Surface DamagePlasma-surface ReactionsSurface RougheningTungsten-based Materials
Tungsten button samples were exposed to He ELMing H-mode plasma in DIII-D using 2.3 MW of electron cyclotron heating power. Prior to the exposures, the W buttons were exposed to either He, or D, plasma in PISCES-A for 2000 s at surface temperatures of 225–850 °C to create a variety of surfaces (surface blisters, subsurface nano-bubbles, fuzz). Erosion was spectroscopically measured from each DiMES sample, with the exception of the fuzzy W samples which showed almost undetectable WI emission. Post-exposure grazing incidence small angle x-ray scattering surface analysis showed the formation of 1.5 nm diameter He bubbles in the surface of W buttons after only a single DIII-D (3 s, ~150 ELMs) discharge, similar to the bubble layer resulting from the 2000 s. exposure in PISCES-A. No surface roughening, or damage, was detected on the samples after approximately 600 ELMs with energy density between 0.04–0.1 MJ m−2.
15
A full tungsten divertor for ITER: Physics issues and design status
R.A. Pitts, S. Carpentier, F. Escourbiac et al. · Journal of Nuclear Materials · 2013 · 776 citations
A design retrospective of the DIII-D tokamak
J.L. Luxon · Nuclear Fusion · 2002 · 526 citations