Composite Interfaces · 2016 · 20 citations · 32 references
Natural SciencesMaterials EngineeringMaterials ScienceMaterials CharacterizationMaterials ChemistryThin FilmsAtomic Force MicroscopyCrystal ChemistryScanning Probe MicroscopyThin-film DepositionThin-film MaterialsAtomic Force Microscopy AnalysisChemical Sensor MaterialsCrystalline StructureFilm ThicknessGrain StructurePyrolysisSpray PyrolysisThin-film Sensor Materials
Na2WO4 films have been grown on Si (1 0 0) and glass substrate using ultrasonic spray pyrolysis. The films are prepared from aqueous solution containing Na2WO4·2H2O at 475 °C temperature and characterized by XRD and SEM techniques and the chemical composition of the films have been verified by EDX and PIXE and its formula Na2WO4 is confirmed by XRD. The evolution of the crystallinity was studied as a function of film thickness ranging from 2500 to 4200 nm, which corresponds to a deposition time from 10 to 30 min, respectively. The crystalline quality was found to improve, where the grain size values increased with increasing thickness. Atomic Force Microscopy (AFM) was used to study the morphology evolution with the deposition time, where porous films were found due to the synthesis parameters, and a better sensing response to gases was developed with increasing thickness. Thus, this study demonstrates the possibility of utilizing Na2WO4 thick films as a sensor element for the detection of ethanol vapor at room temperature, where thicker films exhibit excellent ethanol vapor sensing properties with a maximum sensitivity at 25 °C in air atmosphere with fast response time.
32
John B. Goodenough · Progress in Solid State Chemistry · 1971 · 1.2K citations
Tungsten Oxide-Based Semiconductor Sensor Highly Sensitive to NO and NO2
Morito Akiyama, Jun Tamaki, Norio Miura et al. · Chemistry Letters · 1991 · 290 citations