Silicon Nitride/Silicon Carbide Nanocomposite Materials: I, Fabrication and Mechanical Properties at Room Temperature

Mathias Herrmann, Christian Schuber, Andreas Rendtel, Heinz Hübner

Journal of the American Ceramic Society · 1998 · 126 citations · 27 references

DOIFull text

Open access

Concepts

Abstract

The fabrication of dense Si 3 N 4 /SiC nanocomposite materials that contained 2.5‐30 wt% SiC via gas‐pressure sintering and hot pressing was investigated. The SiC particles originated from admixed commercial SiC powders, SiCN powders produced by plasma synthesis, in situ reaction pyrolysis of carbon‐coated Si 3 N 4 particles, and pyrolysis of a polycarbosilazane‐based SiCN precursor. Based on thermodynamic calculations, criteria for minimum liquid‐phase decomposition during sintering were developed. The best sintering results were obtained for sintering cycles that observed this criteria. Materials that contained plasma‐synthesized SiCN exhibited high strengths (835‐995 MPa) and fracture toughness values (7.4‐7.8 MPam 1/2 ) at room temperature. Post‐sintering thermal treatments led to a strength reduction.

References

27