Fundamental Reflectivity Spectrum of Cd<sub><i>x</i></sub>Hg<sub>1−<i>x</i></sub>Te Crystals from 1.5 to 4 eV

R. R. Gałązka, A. Kisiel

physica status solidi (b) · 1969 · 35 citations · 12 references

Concepts

Abstract

Abstract Reflectivity measurements of solid solutions of Cd x Hg 1− x Te for x from 0.02 to 0.74 and for x = 0 and x = 1 have been performed in the range from 1.5 to 4 eV at the temperature of 315°K. Two maxima in the reflection spectrum were observed. They are interpreted as connected to the transitions E 1 and E 1 + Δ 1 at the Λ‐point of the Brillouin zone. The values of E 1 , E 1 + Δ 1 , and Δ 1 are nonlinear functions of the composition x . The change of the peak position E 1 with the composition between x = 0.00 and 0.10 is nonmonotonous. The reflection spectra for HgTe and CdTe are in a good agreement with previously reported ones.

References

12