Japanese Journal of Applied Physics · 2003 · 37 citations · 4 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor MaterialsSurface ScienceEtching ProcessesOxide SemiconductorsSemiconductor Device MaterialsSemiconductor SurfacesSilicon MaterialsThin Film EtchingCurrent DensityEtch ChemistryEtch MechanismsEtchingOxide Film FormationPatterned SurfacesSurface Current DensitySurface Etching
Commercially available n-type 6H-SiC wafers were etched in aqueous KOH solutions by an electrochemical method. We varied the etching conditions, such as KOH concentration, temperature, UV light illumination and current density, and observed the morphologies of the etched surfaces and etching rates. Etching proceeds with oxide film growth and its peeling off or with continuous dissolution of silicon oxide depending on the conditions. Although the etching under all the conditions roughens the surfaces at a current density of 5 mA/cm2, we obtained the flattest etched surface at a current density of 1 mA/cm2 in 1 wt% KOH concentration at temperature of 50–55°C with UV light illumination. We also fabricated a patterned structure under this etching condition with evaporated Ni metal as a mask.
4