Applied Physics Letters · 1995 · 68 citations · 0 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMaterials ChemistryThin FilmsChemical Vapor DepositionElectrode MaterialsMetal OxidesX-ray CrystallographyX-ray DiffractionExtended X-ray Absorption Fine StructureLeakage CurrentLocal StructureLow-pressure Chemical Vapor DepositionOxide StructureThin Oxide FilmsThin-film OxidesX-ray Absorption Near Edge Structure
Extended x-ray absorption fine structure (EXAFS) above the Ta L3 edge on tantalum oxide capacitor films has been measured. Tantalum oxide films were prepared by low-pressure chemical vapor deposition (CVD) using a Ta(OC2H5)5 and O2 gas mixture. Four kinds of tantalum oxide films were studied: as-deposited (amorphous), N2 annealed (crystalline), dry O2 annealed (crystalline), and O2-plasma annealed (amorphous). From EXAFS analysis, differences in the local structures of tantalum oxide capacitor films, in terms of oxygen deficiency around Ta, were observed in the various annealed films. The leakage current characteristics of tantalum oxide capacitors correspond to the differences in the local structures around Ta.