Chemical Vapor Deposition · 2005 · 20 citations · 23 references
Natural SciencesMaterials EngineeringMaterials ScienceMaterials ChemistrySurface ScienceThin FilmsAmorphous SolidsChemical Vapor DepositionThin-film DepositionThin-film MaterialsX-ray Photoelectron SpectroscopyCrystallinityCrystallinity AnalysisLow-temperature MaterialsPhase Transition TemperatureSubstrate Temperature EffectsSurface ContaminationTitanium MaterialsTitanium Oxides
Titanium dioxide thin films are obtained by CVD on low temperature (60–210 °C) substrates using perpendicular irradiation from a long pulse XeCl excimer laser (308 nm). The precursor, tetra-isopropoxide titanium, is used in an oxygen-containing atmosphere with a total pressure of 10 mbar in the chamber. X-ray photoelectron spectroscopy (XPS) analyses show that the chemical composition of the film, independent of the deposition parameters, is TiO2 with some additional surface carbon contamination. Depending on deposition parameters, the film crystallinity varies between amorphous, anatase, and rutile. Numerical temperature simulations and sample characterization show that the crystalline state of the deposited material evolves from amorphous to anatase to rutile with an increase in the laser-induced temperature. Additionally, substrate temperature and laser repetition rate strongly influence the phase-transition behavior.
23
Raman spectrum of anatase, TiO<sub>2</sub>
T. Ohsaka, Fujio Izumi, Yoshinori Fujiki · Journal of Raman Spectroscopy · 1978 · 2.3K citations
Rutile-type TiO2 thin film for high-k gate insulator
Masaru Kadoshima, Masahiko Hiratani, Yasuhiro Shimamoto et al. · Thin Solid Films · 2003 · 244 citations
Natural Sciences, Materials Engineering, Materials Science +14
Excimer laser processing of indium-tin-oxide films: An optical investigation
T. Szörényi, L.D. Laude, I. Bertóti et al. · Journal of Applied Physics · 1995 · 228 citations