Ferrite Film Recording Surfaces for Disk Recording

R. L. Comstock, E. B. Moore

IBM Journal of Research and Development · 1974 · 22 citations · 6 references

Concepts

Abstract

Ferrite thin films have been prepared using a chemical deposition process; hematite and substituted hematite films were formed by spin coating a diluted solution of the metal nitrates on a substrate and subsequently heating the substrate in air to 300°C to crystallize the film. Magnetic ferrite films were formed by reducing the films in a wet hydrogen atmosphere. Process parameters, which have evolved from studies on spin coating and reduction on 7.62- and 35.56-cm substrates, have been determined that result in desirable magnetic properties. Experimental studies of film composition and morphology are reported. It has been determined both theoretically and experimentally that film thickness near 0.125 µm is optimum for high-density recording with heads with gap lengths of approximately 1 µm spaced about 0.5 µm from the film. A TiO <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</inf> undercoat (0.125 µm) on the Al-Mg alloy substrate was prepared by chemical vapor deposition and resulted in improved magnetic properties. Magnetic properties of the films and magnetic recording performance of disks using Ti and Al substrates with the TiO <inf xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">2</inf> undercoat are reported.

References

6