Journal of Applied Physics · 1990 · 51 citations · 8 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor MaterialsThin FilmsEpitaxial GrowthSemiconductor Crystal GrowthSemiconductor SurfacesSemiconductor Thin FilmsSilicon MaterialsEpitaxial Film GrowthEpitaxial MaterialsEpitaxial Thin FilmsEpitaxial Thin-film GrowthFull Width At Half MaximumPulsed Laser DepositionSiliconSilicon Epitaxy
A new epitaxial oxide, PrO2, has been grown on Si (111) by pulsed laser deposition. X-ray diffraction shows that films are oriented with the PrO2[111] direction parallel to the substrate [111]. The full width at half maximum for the omega rocking curve on the PrO2 (222) peak is as low as 0.75°, while phi scans indicate in-plane epitaxial alignment to better than one degree. In the best quality films, epitaxy is almost pure type-b epitaxy which is characteristic of epitaxial CaF2 on Si. To achieve epitaxy, it is essential to remove the native silicon oxide from the substrate prior to film growth. This is done at room temperature using a wet-chemical hydrogen-termination procedure.
8
Vacuum Deposited Thin Films Using a Ruby Laser
Howard Smith, A. F. Turner · Applied Optics · 1965 · 301 citations
Natural Sciences, Materials Engineering, Materials Science +9