Large remanent polarization of 100% polar-axis-oriented epitaxial tetragonal Pb(Zr0.35Ti0.65)O3 thin films

Hitoshi Morioka, Gouji Asano, Takahiro Oikawa, Hiroshi Funakubo, Keisuke Saito

Applied Physics Letters · 2003 · 76 citations · 14 references

Concepts

Abstract

100% polar-axis (c-axis)-oriented epitaxial Pb(Zr0.35Ti0.65)O3 (PZT) thin films were grown and their large remanent polarization (Pr) was directly measured. Perfectly c-axis-oriented epitaxial PZT thin films were obtained on (100)cSrRuO3//(100)SrTiO3 substrates when the deposition temperature increased to 540 °C together with a decrease in the film thickness down to 50 nm. Polarization–electric-field hysteresis loops were well saturated and had a square shape. The Pr of a 50 nm thick film saturated at 0.9 V, and its value was over 90 μC/cm2; almost independent of the measurement frequency within the range from 20 Hz to 1 kHz. This value was in good agreement with the estimated one from the a- and c-axes mixture-oriented epitaxial PZT film having the same composition taking into account the fact that only the c-axis-oriented domain contributed to the polarization. On the other hand, the coercive field value of a perfectly c-axis-oriented film was 140 kV/cm and almost the same as that of the mixture-oriented one having the same film thickness. These results show that PZT has a large Pr applicable for high-density ferroelectric random access memory.

References

14