Integrated ferroelectrics · 2010 · 10 citations · 18 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials PhysicsDielectric CeramicsDielectricsElectrical ConductivityElectrical Properties Of CeramicsPiezoelectric CeramicsPiezoelectric MaterialsCeramic DielectricsCole-cole PlotDielectric RelaxationElectrical CeramicsFerroelectric RelaxationGrain ResistanceHysteresisTemperature Dependence Of Electrical Properties
Lead-free ceramic samples of [(Na1-xKx)1/2Bi1/2Ti O3] (NKBT) (x = 0.1, 0.15, 0.2, 0.3, 0.45) were prepared by double sintering method and the impedance measurements were carried out in the frequency range of 100 Hz–1 MHz. The Cole–Cole plot show depressed semicircular arcs with spur-like behavior indicate that the temperature dependent dielectric relaxation phenomenon associated with grain boundary conductivity. The temperature variation of grain and grain boundary resistance is found to be linear and obeys Arrhenius law. AC–activation energies, evaluated from the variation of ac-conductivity with inverse temperature plots, were found to decrease with decreasing frequencies and obey the Universal power law. The ferroelectric hysteresis measurements were carried out on poled sample at room temperature and the sample with x = 0.15 composition exhibited the highest Pr value (= 19.2μC/Cm2). The d33 measurements indicate that the sample with x = 0.2 composition has shown the maximum d33 = 85pC/N, when compared with other compositions.
18
Atsushi Sasaki, Tatsuya Chiba, Youichi Mamiya et al. · Japanese Journal of Applied Physics · 1999 · 901 citations
Natural Sciences, Materials Engineering, Materials Science +17
Kazushige Yoshii, Yuji Hiruma, Hajime Nagata et al. · Japanese Journal of Applied Physics · 2006 · 433 citations
Natural Sciences, Materials Engineering, Materials Science +16
J. Kreisel, A. M. Glazer, G. O. Jones et al. · Journal of Physics Condensed Matter · 2000 · 423 citations