Journal of The Electrochemical Society · 1993 · 29 citations · 0 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor MaterialsThin FilmsChemical Vapor DepositionDopingSemiconductor Device MaterialsSemiconductor InterfacesSilicon MaterialsThin Film AnnealingAnnealing Temperature EffectsChemical Vapor Deposition MaterialsDoping In Thin FilmsElectrical PropertiesResistivitySilicon Chemical Vapor DepositionSilicon DopingSilicon Wafers
Compositionally uniform (in depth and in lateral position) chemically vapor deposited films were deposited on 200 mm Si wafers in a single‐wafer reactor using chemistry. A process window was found to produce highly uniform compositions in the range of , regardless of the nucleation surface, or poly‐Si. 900°C annealing in of such films deposited on P‐doped poly‐Si resulted in a uniform reduction of to a value of 2.1 to 2.2. In contrast, as deposited films which are Si‐poor at the interface, were found to develop a high concentration of Si in the middle layer of the annealed structure. The as‐deposited resistivity was found to increase linearly with with a value of ∼750 μΩ · cm for . Upon annealing, the resistivities decreased to values in the range of 80 to 110 μΩ · cm. The as‐deposited films were predominantly in the hexagonal structure of , which transformed to the tetragonal structure upon annealing at temperatures higher than 600°C. As‐deposited stresses were in the range of (1.3 to 1.6) · 1010dyne/cm2, and upon annealing reduced to ∼1 · 1010 dyne/cm2. The films had a very good step coverage even at high aspect ratios and did not crack or peel off upon annealing. The films contained relatively low levels of impurities: and . This systematic study reviews the correlations between the structural, compositional, mechanical, and electrical properties of the as‐deposited and the annealed silicide films.