CdTe/CdS Clusters with “Core−Shell” Structure in Colloids and Films:  The Path of Formation and Thermal Breakup

B. Schreder, Thomas Schmidt, V. Ptatschek, Ulf Winkler, Arnulf Materny, E. Umbach, Martin Lerch, Gerd Müller, W. Kiefer, Lubomír Spanhel

The Journal of Physical Chemistry B · 2000 · 58 citations · 37 references

Concepts

Abstract

A new organometallic “cold−slow” route to strongly fluorescing CdTe/CdS (core−shell) colloids and transparent films is presented. Based on the optical absorption, fluorescence, FTIR, micro-Raman, XPS, and XRD data collected on these nanostructures before and after thermal annealing, a mechanistic path of the core−shell formation and thermal break up is proposed and discussed. The processing of the CdTe/CdS nanostructures starts with 0.5 M tributylphosphine (TBP) stabilized CdS colloid in dichloromethane as a solvent. This yellow colloidal oil composed of 3−4 nm CdS clusters is reacted with liquid Bis(trimethylsilyl)-telluride (TMS 2 Te) in the presence of excess insoluble CdCl 2 salt. During this reaction, a rapid chalcogen atom exchange occurs within a few seconds which produces a new CdTe “core”. The expelled sulfide reacts slowly with the CdCl 2 salt to form new CdS clusters after several hours. Furthermore, this “CdS-formation-driven CdCl 2 salt dissolution” activates a strong green-yellow fluorescence indicating a possible evolution of a “core−shell”-like CdTe/CdS structure. Thermal sintering of the subsequently prepared CdTe/CdS films between 100 and 200 °C completely suppresses the fluorescence and initiates CdTe cluster growth, reflecting a high thermal sensitivity of the “core−shell” interfaces. By further raising the sintering temperature to 300−400 °C, the TBP ligands are released and, consequently, bare CdS- and CdTe nanocrystals, as well as ternary nanocrystalline CdTe x S 1 - x phases, start forming. Above 400 °C, the CdTe part of the nanostructures sublimates, yielding (111)-oriented CdTe films.

References

37