TU/e Research Portal (Eindhoven University of Technology) · 2010 · 23 citations · 0 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor DevicesSemiconductor MaterialsSemiconductor Device MaterialsSemiconductor SurfacesSilicon MaterialsSolar CellsSurface ModificationSurface PassivationDeposition TechniquesPassivationPassivation Of SemiconductorsReactive SputteringSilicon Solar CellsSilicon WafersSurface Passivation LayersSurface Recombination
We present independently confirmed efficiencies of 21.4% for PERC cells with plasma-assisted atomic- layer-deposited (plasma ALD) Al2O3 rear passivation and 20.7% for cells with thermal ALD-Al2O3. Additionally, we evaluate three different industrially relevant techniques for the deposition of surface-passivating Al2O3 layers on 1- Ωcm p-type silicon wafers, namely high-rate spatial ALD (spatial ALD), plasma-enhanced chemical vapour deposition (PECVD) and reactive sputtering. Using spatial ALD and PECVD, surface recombination velocities (SRVs) below 10 cm/s are obtained. Sputtered Al2O3 layers still provide an SRV of 35 – 70 cm/s. Despite their lower passivation quality compared to the Al2O3 films deposited by spatial ALD and by PECVD, we demonstrate that the sputtered Al2O3 layers are still suitable for the fabrication of 20.1% efficient PERC cells. After firing at ~800°C in a conveyorbelt furnace the SRV provided by the Al2O3 films deposited by spatial ALD is still below 20 cm/s, indicating an excellent firing stability. Both PECVD and sputtered Al2O3 passivation layers degrade to SRVs larger than 100 cm/s after firing. Hence, the firing stability of PECVD and – in particular – sputtered Al2O3 needs further optimisation.