Natural SciencesMaterials EngineeringMaterials ScienceMetallic MaterialsMetallurgySurface ScienceCathode MaterialsPlasma-surface InteractionsPowder MetallurgyPowder ProcessingSinteringSurface PhysicsActivated SinteringGlow Discharge TreatmentPorositySintering BehaviorSintering KineticsSurface PorositySurface Porosity ControlSurface Sputtering
Samples of unalloyed iron powder were compacted and sintered in an abnormal glow discharge, generated in a gas mixture of 80% Ar + 20% H2 by using a pulsed power source. The samples were placed on a holder, acting as the discharge cathode, and were heated by the bombardment of ions, strongly accelerated in the cathode sheath. Sintering was performed at temperatures of 1173, 1273 and 1373 K for 30 min, varying the voltage applied to the cathode from 400 to 700 V and pressure ranging from 470 to 2650 Pa. It is shown that the kinetic energy of ions striking the sample surface increased approximately three times, when the voltage changed from 400 to 700 V, with a corresponding reduction of surface porosity. The surface sealing is related to the ion bombardment, which produced a high mobility of surface atoms and consequent enhanced diffusion as well as sputtering and condensation on the concave surface, resulting in an activation of surface sintering.
30
Introduction to Powder Metallurgy
Materials Characterization · 1995 · 194 citations
Natural Sciences, Materials Engineering, Materials Science +12
Book Review: INTRODUCTION TO POWDER METALLURGY
D. S. Coleman · Surface Engineering · 1994 · 193 citations
Natural Sciences, Materials Engineering, Materials Science +12