Ultrasonic measurements of the elastic moduli of ultradrawn polyoxymethylene

W. P. Leung, C. L. Choy, Koichi Nakagawa, T. Konaka

Journal of Polymer Science Part B Polymer Physics · 1987 · 19 citations · 18 references

Concepts

Abstract

Abstract We have employed an ultrasonic method to measure from −40 to 60°C the five independent elastic moduli C 11 , C 13 , C 33 , C 44 , and C 66 of polyoxymethylene with draw ratio λ from 1 to 26 prepared by continuous drawing under microwave heating. The elastic moduli are controlled by three major factors: molecular orientation in the crystalline regions, fraction of noncrystalline taut tie molecules, and void content. The steep rise in the axial extensional modulus C 33 and axial Young's modulus E 0 with increasing draw ratio results from the alignment of chains in the crystalline blocks and an increase in the number of disordered taut tie molecules. Below the γ relaxation (located at 0°C at our measurement frequency of 10 MHz), these two factors also give rise to a slight decrease in the transverse extensional modulus C 11 , Young's modulus E 90 and shear modulus C 66 . At high temperature where the amorphous regions have very low modulus, the stiffening effect of taut tie molecules becomes dominant, leading to an increase in all moduli as λ increases from 1 to 10. At higher λ the void fraction increases appreciably, causing small decreases in E 90 , C 11 , and C 66 at all temperatures.

References

18