Journal of Applied Physics · 2006 · 24 citations · 6 references
Natural SciencesMaterials EngineeringMaterials ScienceMagnetic MaterialsMicrofabricationThin FilmsFerromagnetic MaterialsFerromagnetismMagnetic AnisotropyMagnetic Thin FilmsMagnetization ProcessesThin Film Magnetic PropertiesAnisotropy In Thin FilmsCoercivityCoercivity EnhancementDeposition RateMagnetic Anisotropy EngineeringPulsed Laser DepositionThin Film FerromagnetsThin-film Magnetic Materials
The interceptive deposition method (IDM) was applied to the high-speed pulsed laser deposition (PLD) method with a substrate heating system, and it was clarified that anisotropic Nd-Fe-B thick-film magnets can be obtained under a high deposition rate larger than 20–50μm∕h. The obtained coercivity, remanence, and (BH)max values of a film were 577kA∕m, 0.90T, and 118kJ∕m3, respectively. In addition, we succeeded in increasing the thickness up to 90μm for an anisotropic Nd-Fe-B film magnet by using IDM.
6
Anisotropic Nd–Fe–B thin-film magnets for milli-size motor
Shinji Yamashita, J. Yamasaki, M. Ikeda et al. · Journal of Applied Physics · 1991 · 172 citations · Full text
Natural Sciences, Materials Engineering, Materials Science +17