Nd–Fe–B Thin Films with Perpendicular Magnetic Anisotropy and High Coercivity Prepared by Pulsed Laser Annealing

Takashi Okuda, Akinori Sugimura, Osamu Eryu, L.K.E.B Serrona, Nobuyasu Adachi, I. Sakamoto, A. Nakanishi

Japanese Journal of Applied Physics · 2003 · 19 citations · 2 references

Concepts

Abstract

Amorphous, as-deposited Nd–Fe–B films prepared by RF-sputtering were annealed by irradiating pulsed KrF excimer laser (248 nm). A pulse of 20 ns in width and 4 kJ/m2 in power density was irradiated onto a 2 µm-thick as-deposited film kept at 400°C. It is observed that, by a single shot of the pulse, Nd2Fe14B Φ phase crystallized with prominent texturing of c-axis along the film normal. Annealed films showed excellent magnetic characteristics; Ms=0.978 T, Mr=0.906 T, iHc=1272 kA/m, and (BH)MAX=161 kJ/m3. This process is also found to be successfully applicable to a 20 µm-thick film. Using 2 µm-thick as-deposited film kept at 400°C, micro-magnet patterns of 100 µm in width and 1–2 mm in length were fabricated by irradiating a 20-ns pulse shot through a patterned mask. The patterned area revealed that magnetizations are directed along the film normal with coercivity higher than 1200 kA/m.

References

2