Durability of Oilwell Cement Formulations Aged in H2S-Containing Fluids

Éric Lécolier, Alain Rivereau, N. Ferrer, A. Audibert, X. Longaygue

2006 · 26 citations · 4 references

Concepts

Abstract

Abstract In the next few decades, the production of oilfields with high contents of associated sour gases will increase. For instance, we estimate that 40% of the world remaining gas reserves contain more than 2% of CO2 and/or more than 100 ppm of H2S. Therefore, investigations on technologies to produce such fields are of utmost importance. Due to the presence of corrosive gas, special attention has to be paid to the design of well materials (casing, cementing materials). Corrosion of steel due to acid gas containing brines is well documented in the literature, and to a lesser extent, data about the degradation by wet CO2 or wet H2S can be found. For cementitious materials, one can find abundant literature dealing with deterioration of cement pastes due to CO2 environment. Published data on degradation mechanisms of cement-based materials exposed to H2S environments are more scarce. This paper addresses the problem of durability of oilwell cement in different hydrogen sulphide environments. Different periods of time can be identified in the lifetime of the wells: the production period (about 20 to 40 years), the post-abandonment period (some tens of years following the permanent well abandonment) and the abandonment period (several centuries). For each period of time, cementing materials (primary cementing, plugs) are in contact with different types of fluids. Therefore, to correctly assess the behaviour of oilwell cement, ageing tests have to be carried out in fluids representative of these different periods of time. In this paper, we present the methodology implemented under HP/HT conditions for ageing tests of materials in H2S-containing fluids and results obtained on cement-based materials. Main physico-chemical degradation mechanisms of cement-based materials due to H2S are identified using different characterization techniques. Depending of the nature of the fluid in contact with cementitious materials, severe degradation can occur with dramatic impairment of macroscopic properties.

References

4