Sensitization of Austenitic Stainless Steels II. Commercial Purity Alloys

R. A. Mulford, E. L. Hall, C. L. Briant

CORROSION · 1983 · 76 citations · 22 references

Concepts

Abstract

This paper presents a study of the effects of nitrogen and molybdenum on the sensitization of commercial purity type 304 and 316 stainless steels. The modified Strauss test (ASTM-A262-E) is used to determine the degree of sensitization of the steels, and Auger spectroscopy and analytical electron microscopy are used to study the chemistry of grain boundaries and the crystallography and chemistry of grain boundary phases. The corrosion data from different alloys are considered in terms of effective chromium content. The corrosion behavior of commercial purity 304 and 316 alloys is found to be inferior to the corresponding high-purity alloys. The Auger data indicates that this is due to the segregation of phosphorus to the grain boundaries. Nitrogen has a beneficial effect on the behavior of type 304 stainless steel, but the improvement due to this element is generally less than in high-purity alloys. Molybdenum additions strongly improve the corrosion behavior by increasing the amount of chromium depletion necessary for sensitization. Quantitative X-ray microanalysis in the analytical electron microscope is used to measure the elemental composition at grain boundaries in the vicinity of carbides in sensitized specimens. Evidence is found that the depletion of molybdenum plays an important role in the sensitization of type 316 stainless steel. In type 316L with high levels of nitrogen, several different phases are found at the grain boundaries, which affects the degree of chromium depletion at these boundaries.

References

22