Materials Research · 2001 · 90 citations · 11 references
Natural SciencesChemistryMaterials ScienceCatalysisPolymer ChemistrySpectroscopyGelsInfrared SpectroscopyFourier TransformGelationPolymer GelationSilicate ChemistrySol-gel MaterialsSol-gel ProcessingStabilizationTime-dependent Chemical Evolution
In this work we investigated the influence of formamide on the acid-catalyzed sol-gel process by Fourier transform infrared spectroscopy (FTIR). Three silica sols were studied: Sol catalyzed with nitric acid without formamide, sol catalyzed with nitric acid containing formamide and sol catalyzed with a mixture of nitric acid and hydrofluoric acid and modified with formamide. Following the time evolution of both the Si-(OH) stretching vibration at around 950 cm-1 and the Si-O-(Si) vibration between 1040 cm-1 and 1200 cm-1 we were able to describe the structural evolution of each sol. The curve of evolution of Si-(OH) stretching vibration corresponding to sol A has a simple asymptotic evolution. In the case of formamide containing sol, we observed a two-step structural evolution indicating that for the system containing formamide the polymerization goes through a temporary stabilization of oligomers, which can explain the non-variation of the Si-O(H) bond wavenumber for a certain time. Gelation times were of several days for gels without formamide and few hours for gels containing additive. The presence of additive resulted in a highly interconnected gel.
11
Kr Iler · Medical Entomology and Zoology · 1979 · 5K citations
M. Schraml-Marth, K.L. Walther, Alexander Wokaun et al. · Journal of Non-Crystalline Solids · 1992 · 183 citations
Natural Sciences, Materials Engineering, Materials Science +15