ISIJ International · 2013 · 72 citations · 16 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsPhase TransformationsFerrimagnetic MaterialsIron OxidesMineral ChemistryMineral GenesisOre MineralogySinteringBondingFerrite FormationFerritesIn Situ X-ray DiffractionMineral Phase AnalysisPowder DiffractionPowder X-ray DiffractionX-ray Diffraction Analysis
The formation mechanisms of the complex Ca-rich ferrite phase SFCA-I, an important bonding material in iron ore sinter, during heating of synthetic sinter mixtures in the temperature range 298–1623 K in air and at pO2 = 5 × 10–3 atm, were determined using in situ X-ray powder diffraction. In air, the initial formation of SFCA-I at ~1438 K (depending on composition) was associated with reaction of precursor phases Fe2O3, CaO·Fe2O3, SiO2, amorphous Al-oxide and a CFA phase of approximate composition 71.7 mass% Fe2O3, 12.9 mass% CaO, 0.3 mass% SiO2 and 15.1 mass% Al2O3. At temperatures above ~1453 K, the decomposition of another phase, γ-CFF, resulted in the formation of additional SFCA-I. At lower oxygen partial pressure the initial formation of SFCA-I occurred at similar temperatures and was associated with reaction between similar phases as its formation in air. However, the decomposition of γ-CFF did not result in the formation of additional SFCA-I, with the maximum SFCA-I concentration (25 mass%) lower than the values attained in air (54 and 34 mass%). Hence, more oxidising conditions appear to favour the formation of the desirable SFCA-I phase.
16
The structure of calcium ferrite
B. F. Decker, J. S. Kasper · Acta Crystallographica · 1957 · 248 citations · Full text
Nathan A. S. Webster, Mark I. Pownceby, Ian C. Madsen et al. · Metallurgical and Materials Transactions B · 2012 · 194 citations
Natural Sciences, Materials Engineering, Materials Science +16