Journal of Applied Physics · 1957 · 46 citations · 3 references
Natural SciencesElectrical EngineeringMaterials ScienceElectrochemistryElectronic MaterialsThin FilmsDefects In Electronic MaterialsDielectric CeramicsDielectricsElectrical CharacterizationElectrical ConductivityThin Film Electrical PropertiesBreakdown MechanismsBreakdown StrengthDielectric BreakdownDielectric StrengthElectrical BreakdownField EmissionFilm ThicknessMoisture Content
Dc breakdown studies on Mylar film show that defects cause a decrease in dielectric strength with decreasing film thickness at room temperature but not at −180°C. The breakdown at defects is associated with moisture content. Using self-healing electrodes to eliminate weak areas, a dc dielectric strength of 6 Mv/cm is found, independent of film thickness. Prebreakdown current measurements indicate ionic currents which are fairly uniform throughout a sample, and field emission currents localized at incipient breakdown points. Breakdown probably occurs as a result of local heating by field emission currents.
3
Arthur R. von Hippel, S. O. Morgan · Journal of The Electrochemical Society · 1955 · 1.1K citations
Natural Sciences, Chemistry, Physics +17