Hydrogen-bonding configuration effects on the optoelectronic properties of glow discharge a-Si<sub>1−<i>x</i></sub>Ge<sub><i>x</i></sub>:H with large<i>x</i>

Y. Bouizem, A. Belfedal, J.D. Sib, A. Kebab, L. Chahed

Journal of Physics Condensed Matter · 2007 · 16 citations · 30 references

Concepts

Abstract

The optical and structural properties of hydrogenated amorphous silicon–germanium (a-Si1−xGex:H) films, deposited at high growth rate by radio-frequency (RF) glow discharge on the powered electrode in a conventional parallel plate reactor, were investigated by infrared transmission measurements, standard optical transmission measurements and the photothermal deflection spectroscopy (PDS) method. By varying the electrode gap spacing, D, from 3.2 to 0.8 cm, and keeping all others parameters of the plasma constant, a gradual change in the hydrogen-bonding configurations was observed. The effects of this change on the structure of the material, on the optical gap, and on the midgap density are investigated and discussed at high fixed composition (x = 0.8) and at constant total bonded hydrogen content (CH(at.%) = 8.5). The optical gaps (1.16 eV ≤ET≤1.22 eV) of the films are less than those of conventional films, reported in the literature. The level of absorption at energies bellow the Urbach tail decreases with D and reaches an optimum at D = 0.8 cm. The disorder parameter (E0v≈46 ± 1 meV) and the level of absorption in optimized samples are of the same order as those of device-quality a-Si:H films. It is suggested that the remarkable improvement of the electronic properties of the alloys is mainly due to the incorporation of the hydrogen in the bulk of the material as Ge–H and Si–H bonds, with a preferential attachment to Ge rather than to both Ge and Si.

References

30