Strength and Microstructure of Silicon Nitride Ceramics Brazed with Nickel‐Chromium‐Silicon Alloys

Ali Mohammad Hadian, R. A. L. Drew

Journal of the American Ceramic Society · 1996 · 32 citations · 9 references

Concepts

Abstract

Joining of sintered Si 3 N 4 was performed using a high‐temperature brazing technique. Ni‐based brazing alloys having the same Ni:Cr ratio as AWS BNi‐5 (Ni·18Cr·19Si (at. %)) but different Si content were used as the brazing filler metals. Joining experiments were performed at 1220°C under a N 2 partial pressure of 15 Pa for different times between 5 to 15 min. The highest room‐temperature four‐point bend strength of the joints was 115 MPa, whereas 220 MPa was achieved when the joints were tested at 900°C. The high strength of the experimental joints was attributed to the reduction in residual stresses and formation of a CrN reaction layer at the ceramic/filler metal interface.