IEEE Transactions on Magnetics · 1989 · 54 citations · 3 references
Natural SciencesMaterials EngineeringMaterials ScienceMagnetic MaterialsMetallic MaterialsMetallurgyFerromagnetic MaterialsFerromagnetismMagnetic Properties Of SolidsMagnetism In SolidsPermanent MagnetsRemanent MagnetizationComposition TuningFerrite MagnetsMagnetic CoercivityMagnetic Materials CharacterizationMagnetic PropertiesMagnetic Property CharacterizationMagnetitePowder Metallurgy Of Magnets
The magnetic properties of Sm/sub 2/(Co,Fe,Cu,Zr)/sub 17/ magnets were improved by increasing the Fe content without raising the Zr content. With increasing Fe content, the remanence rises monotonically while the intrinsic coercive force drops sharply for 0.27<v<0.29 and then increases for 0.30<v<0.33 in Sm(Co/sub bal/Fe/sub v/Cu/sub 0.056/Zr/sub 0.02/)/sub 7.546/. For the nominal composition Sm(Co/sub 0.612/Fe/sub 0.316/Cu/sub 0.052/Zr/sub 0.02/)/sub 7.73/, most magnets developed (BH)/sub max/=31-33 MGOe while some reached 33-34 MGOe. Still higher Fe contents may result in further improvement of Sm/sub 2/TM/sub 17/ magnets.<<ETX>>
3
AEM studies of Sm:Co 2:17 permanent magnet alloys
Bing Zhang, J.R. Blachère, W.A. Soffa et al. · Journal of Applied Physics · 1988 · 21 citations
Natural Sciences, Materials Engineering, Materials Science +16