The Journal of Physical Chemistry B · 2006 · 94 citations · 28 references
Natural SciencesChemistryMaterials ScienceSpectroscopySurface ChemistrySurface ScienceOxidation ReactionsRaman SpectroscopySilicon MaterialsSurface KineticsSurface OxidationSurface PhysicsChemical EtchingEtch RateIntermediate Species ConcentrationSiliconSilicon EtchingSilicon OxidationWet Chemical EtchingWet Etching
The role of intermediate species generated during wet chemical etching of silicon in a HF-rich HF/HNO3 mixture was studied by spectroscopic and analytical methods at 1 degrees C. The intermediate N2O3 was identified by its cobalt blue color and the characteristic features in its UV-vis and Raman spectra. Furthermore, a complex N(III) species (3NO+.NO3-) denoted as [N4O6(2+)] is observed in these solutions. The time-dependent decay of the N(III) intermediates, mainly by their oxidation at the liquid-air interface, serves as a precondition for the study of the etch rate as function of the intermediate concentration measured by Raman spectroscopy. From a linear relationship between etch rate and [N4O6(2+)] concentration, NO+ is considered to be a reactive species in the rate-limiting step. This step is attributed to the oxidation of permanent existing Si-H bonds at the silicon surface by the reactive NO+ species. N2O3 serves as a reservoir for the generation of NO+ leading to a complete coverage of the silicon surface with reactive species at high intermediate concentrations. As long as this condition is valid (plateau region), the etch rate is constant and yields a smooth silicon surface upon completion of the etching. If the N2O3 concentration is insufficient to ensure a coverage of the Si surface by NO+, the etch rate decreases linearly with the N2O3 concentration and results in a roughening of the etched silicon surface (slope region).
28