Thermal Expansions from 2 to 40°K of Ge, Si, and Four III-V Compounds

Paul Whitney Sparks, C. A. Swenson

Physical Review · 1967 · 148 citations · 29 references

Concepts

Abstract

Linear thermal-expansion data are given for Ge, Si, GaAs, GaSb, InAs, and InSb at temperatures from 1.89\ifmmode^\circ\else\textdegree\fi{}K to approximately 40\ifmmode^\circ\else\textdegree\fi{}K. The data were obtained using a variable transformer as a sensor and are absolute in sample length changes. At the lowest temperatures, the length-change data for 10-cm samples exhibit a scatter of \ifmmode\pm\else\textpm\fi{}0.02 \AA{} (or \ifmmode\pm\else\textpm\fi{}2\ifmmode\times\else\texttimes\fi{}${10}^{\ensuremath{-}11}$ in $\frac{\ensuremath{\Delta}L}{{L}_{0}}$). The precision at all temperatures (within this limitation) is 2%. All of these substances show a positive thermal-expansion coefficient which is proportional to ${T}^{3}$ at low temperatures, while at higher temperatures the expansion coefficient becomes negative. The linear thermal-expansion data are used to calculate the temperature dependence of the Gr\"uneisen constants for each of these. With the exception of Si, a correlation exists between the Debye temperature and both the magnitude of ${\ensuremath{\gamma}}_{0}$ and the shape of the $\ensuremath{\gamma}$-versus-$T$ curve. There is discrepancy between our observed values of ${\ensuremath{\gamma}}_{0}$ for Ge and Si (0.66 and 0.42, respectively) and those calculated from the 77\ifmmode^\circ\else\textdegree\fi{}K third-order elastic-constant data. The reason for the discrepancy (which is a factor of 2 for Si) is not known.

References

29