Preparation and Magnetic Characteristics of Chemically Deposited Cobalt for High-Density Storage

R. Fisher, W. H. Chilton

Journal of The Electrochemical Society · 1962 · 63 citations · 0 references

Concepts

Abstract

Chemically reduced cobalt coatings on a nonconductive substrate (Mylar) have been prepared which are suitable for high‐density data storage applications. The influence of deposition parameters such as temperature, total solution concentration of cobalt plus hypophosphite ion, and pH on the hysteresis properties and surface characteristics of chemically reduced cobalt was investigated. The deposits are isotropic in nature so that no preferred direction of magnetization exists in the plane of the film. The coercive force of the deposits is an inverse function of the thickness, and the squareness (Br/Bm) is primarily dependent on the thickness. The saturation magnetization may vary from 8,000 to 14,000 gauss depending on the impurity content of the deposit. A typical deposit has a coercive force of 360 oersteds at a thickness of 13,000Aå. The deposits are crystalline as evidenced by x‐ray diffraction patterns and electron microscopy in contrast to chemically reduced nickel deposits which are reported to be amorphous. Recording characteristics of the deposits are similar to those of commercial oxide recording tapes.