Optical Properties of Tantalum Oxide Films on Silicon

A. G. Revesz, J. H. Reynolds, J. F. Allison

Journal of The Electrochemical Society · 1976 · 21 citations · 0 references

Concepts

Abstract

Tantalum oxide films on silicon were prepared by thermal oxidation of vacuum,deposited Ta films. The optical absorption of these noncrystall ine films resembles closely that of crystall ine Ta2Os, indicating a strong similarity in their short-range order structures. For given oxidation conditions, the re-fractive index of the oxide films increases from,,-1.93 to 2.34 as the thickness increases from 12.5 to 111.7 nm. For a given tantalum film thickness, higher oxidation temperatures result in thicker oxides of lower refractive index. Additional oxide growth occurs during postoxidation heat-treatment in oxy-gen while the refractive index decreases. The refractive index of a given oxide film increases from the Si/oxide interface toward the outer surface, e.g., from 2.08 to about 2.4. These phenomena re attributed to the incorporation of silicon into the Ta oxide during its growth. However, the estimated amount of silicon in the oxide is not sufficient o explain the observed values if it is assumed that the lowering of the refractive index is due simply to mixing Ta20~