EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsSemiconductor DevicesSemiconductor MaterialsConducting PolymersOrganic Electronic MaterialsOrganic SemiconductorsPhotovoltaic DevicesPhotovoltaic MaterialsSolar CellsBulk Heterojunction Solar CellsCarrier MobilityCarrier Mobility MeasurementsCharge Carrier MobilityOrganic Photovoltaic CellsOrganic Solar CellsPhotocurrent GenerationPower Conversion
The initial performance and subsequent degradation of inverted polymer solar cells [indium–tin oxide/titanium oxide (TiO x )/[6,6]-phenyl C 61 butyric acid methyl ester (PCBM): regioregular poly(3-hexylthiophene) (P3HT)/poly(3,4-ethylenedioxylenethiophene):poly(4-styrene sulfonic acid)/Au, TiO x cell] are studied by photocurrent–voltage measurements as well as ac impedance spectroscopy (IS) and carrier mobility measurements. The TiO x cells containing a P3HT:PCBM layer prepared from a solution of chlorobenzene (CB) showed a maximum power conversion efficiency (PCE) of 2.23%. In contrast, the TiO x cells containing a P3HT:PCBM layer prepared from a solution of 1,2,3,4-tetrahydronaphthalene (tetralin) containing 2 vol % 1,8-octanedithiol (ODT) exhibited a maximum PCE of 2.92%. However, after exposure to light irradiation for 100 h, the maximum PCE of the tetralin:ODT cell decreased to 68% of its initial value. On the other hand, over 96% of the maximum PCE was maintained in the CB cell after 100 h of irradiation. The IS measurement results suggest that the degradation of the Tetralin:ODT cell was caused by a morphological change of the P3HT:PCBM layer that made efficient photoinduced charge separation difficult.
30